Guide
Stainless steel and alloy grade selection guide
How to choose between 304L, 316L, 321, 904L, duplex, super duplex, 6Mo, Monel, Inconel, Hastelloy, copper-nickel and titanium for fittings and flanges.
Method
Start with the medium and the temperature
Choosing a grade is a balance of corrosion resistance, strength, temperature, fabrication and cost. Begin with the medium (including trace chlorides), its concentration and temperature, the design pressure and any code or client requirements. Then pick the lowest-cost grade that is proven for that duty.
For chloride environments a useful comparison is the pitting resistance equivalent number (PREN = %Cr + 3.3 × %Mo + 16 × %N). Higher numbers mean better resistance to pitting. Typical values are about 24 for 316L, 35 for 904L and 2205 duplex, and above 40 for super duplex and 6Mo grades.
Reference
Grade families at a glance
| Family | Examples | Strengths | Limits |
|---|---|---|---|
| Austenitic stainless | 304L, 316L, 321, 347, 310S | Formable, weldable, good general corrosion resistance | Chloride pitting and stress corrosion cracking |
| High-alloy austenitic | 317L, 904L, 254 SMO (6Mo) | Better acid and chloride resistance | Cost; welding needs care |
| Duplex | 2205 (S31803 / S32205) | About twice the strength of 316L; chloride SCC resistance | Limited to about 300 °C |
| Super duplex | S32750, S32760 | Seawater pitting resistance and high strength | Qualified welding; cost |
| Nickel alloys | Monel 400, Inconel 600 / 625, Alloy 20, C276 | Severe acids, high temperature, seawater | Cost; availability |
| Copper alloys | CuNi 90/10, 70/30, admiralty brass | Seawater and biofouling resistance | Velocity limits; sulphides |
| Titanium | Grade 2, Grade 5 | Outstanding in seawater and chlorides | Cost; reducing acids |
Materials
Browse by material
Stainless steels
Duplex, super duplex and 6Mo
Copper alloys and titanium
Carbon and alloy steel, aluminium
Pipes, tubes, bars and plates
Polymers and others
FAQ
Frequently asked questions
Is 316L always better than 304L?
For chlorides and many chemicals, yes. For plain water and many food uses, 304L performs just as well at a lower cost.
When do I need a stabilised grade such as 321 or 347?
When the steel will spend time between about 425 °C and 815 °C in service or during fabrication, where unstabilised grades can become sensitised to intergranular corrosion.
Can different grades be welded together?
Yes, with a suitable filler metal and procedure, but check galvanic effects in conductive media and any code limits.
Next step
Tell us what you need
Part number, size, material or a full list: send it and get a clear quotation.